Industrial Consultancy & Sponsored Research (IC&SR) , IIT Madras

A Method for Producing High Performance Cryorolled Ultrafine Grained Bimetallic Composite Sheets

Categories for this Invention

Technology: Cryorolled Ultrafine Grained Bimetallic Composite Sheets

Category: Advanced materials

Industry: Electronic System & Design Manufacturing (ESDM)

Application: Electrical and Electronics Industries.

Market: The global market size of projected to grow  from USD 6.67 billion in 2018 to USD 12.17 billion by 2027, at a CAGR of 6.92%.

Image Gallery

Problem Statement

  • Bimetals, particularly Al/Cu bimetals, are widely used in various industries due to their hybrid properties. They are particularly popular in electrical components like cables and connectors.
  • Traditional manufacturing methods like diffusion bonding, roll bonding, explosive welding, and ultrasonic welding are suitable for Al/Cu bimetallic joining. However, intermetallic formation in these processes can reduce electrical conductivity and properties.
  • Roll bonding is the most popular technique for producing Al/Cu bimetallic sheets due to its ease of use and process flexibility.
  • A new, technologically advanced manufacturing route is needed to achieve superior interface, ultra-high bond strength, and excellent mechanical properties.

Technology

METHOD:

  • The method comprising partitioning at least one aluminium plate and at least one copper plate with predetermined thicknesses and machined to the desired size
  • Subjecting the aluminium and copper plates to homogenization through a heat treatment process
  • Subjecting the aluminium and copper plates to cryogenic-soaking process to for a predefined time period
  • Subjecting the aluminium and copper plates to multi-pass cryorolling with thickness reduction to develop cryorolled aluminium and copper sheets
  • Subjecting the cryorolled copper sheet to a short thermal treatment followed by water quenching
  • Performing surface preparation on the cryorolled aluminium sheet and copper sheet involving at least one of drilling, degreasing, scratch brushing and riveting
  • Subjecting surface prepared sheets to roll bonding with a thickness reduction to develop ultrafine grained aluminium/copper bimetallic sheets
  • Subjecting the ultrafine grained aluminium/copper bimetallic sheets to asymmetrical rolling
  • Subjecting the asymmetrically rolled ultrafine grained aluminium/copper bimetallic sheets to heat treatment for a short period of time to produce high performance cryorolled ultrafine grained bimetallic composite sheets

Key Features / Value Proposition

Temperature

  • Cryorolling is performed at a very low of approximately minus (-) 196°C.

Soaking

  • The aluminium and copper plates in liquid nitrogen for minimum 15 mins before each pass.

A 2-High rolling mill

  • Approximately 125 mm roll diameters and the rolling is carried out at approximately 6 to 8 rpm.

Thickness reduction

  • 80% during multi-pass cryorolling with an average grain size of approximately 1 µm

Short thermal treatment

  • 250°C to 450°C for a time period of 5 to 15 minutes.

Roll bonding

  • a thickness reduction range of approximately 55 to 60%.

Roll Spec

  • Roller diameter 300 mm
  • Rolling speed 4-6 rpm and
  • Rolling load 30-45 tons

Speed ratio

  • Approximately 1.1 to 1.5 on a 2-high rolling.

Bond strength

  • Approximately 24 to 28 N/mm and
  • Excellent strength-ductility synergy
  •  (tensile strength of approximately 200MPa and
  • Total ductility of ( 35 to 40%) approximately .

Questions about this Technology?

Contact For Licensing

sm-marketing@imail.iitm.ac.in
ipoffice2@iitm.ac.in

Research Lab

Prof. Sushanta Kumar Panigrahi

Department of Mechanical Engineering.

Intellectual Property

  • IITM IDF Ref. 2492
  • Patent No: IN 528430

Technology Readiness Level

TRL-4

Experimentally validated in Lab;